PP Copolymer SAXALEN™ PPC345G30 SAX AUSTRIA
0
- ویژگیها:Filler glass fiber reinforced material 30% filler by weight
برگه داده فنی
| impact performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 9.0 kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 50 kJ/m² |
| -30°C | ISO 179/1eU | 39 kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 13 kJ/m² |
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 50 kJ/m² |
| -30°C | ISO 180/1U | 40 kJ/m² | |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 14 kJ/m² |
| -30°C | ISO 180/1A | 9.0 kJ/m² |
| mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
|---|---|---|---|
| bending strength | ISO 178 | 105 MPa | |
| Bending modulus | ISO 178 | 4500 MPa | |
| Tensile strain | Break | ISO 527-2/5 | 4.0 % |
| tensile strength | Break | ISO 527-2/5 | 55.0 MPa |
| Tensile modulus | ISO 527-2/1 | 5200 MPa |
| thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
|---|---|---|---|
| Vicat softening temperature | ISO 306/B120 | 118 °C | |
| Hot deformation temperature | 1.8MPa,Unannealed,60.0mmSpan | ISO 75-2/A | 127 °C |
| Physical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
|---|---|---|---|
| Melt Volume Flow Rate (MVR) | 230°C/2.16kg | ISO 1133 | 15.0 cm³/10min |
| density | ISO 1183 | 1.08 g/cm³ |