برگه داده فنی
شرایط آزمون | روش آزمون | نتیجه آزمون | |
---|---|---|---|
density | ASTM D792 | 1.70 g/cm³ | |
melt mass-flow rate | 297°C/5.0kg | ASTM D3159 | 4.0 g/10min |
Water absorption rate | 24hr | ASTM D570 | 7E-03 % |
tensile strength | 23°C | ASTM D3159 | 47.0 MPa |
elongation | 断裂,23°C | ASTM D3159 | 300 % |
Flexural modulus | 23°C | ASTM D790 | 1200 MPa |
compressive strength | ASTM D695 | 38.0 MPa | |
Impact strength of cantilever beam gap | 23°C | ASTM D256 | NoBreak |
maximum service temperature | UL 746 | 150 °C | |
Volume resistivity | ASTM D257 | 1E+17 ohms·cm | |
dielectric strength | 0.250mm | ASTM D149 | 70 kV/mm |
dielectric constant | 23°C,1MHz | ASTM D1531 | 2.50to2.60 |
Dissipation Factor | 23°C,1MHz | ASTM D1531 | 7.2E-03 |
arc resistance | ASTM D495 | 122 sec | |
Limiting Oxygen Index | ASTM D2863 | 30to32 % | |
Shore hardness | 邵氏D | ASTM D2240 | 72 |
melting temperature | ASTM D3159 | 255to280 °C | |
Linear coefficient of thermal expansion | MD:0到100°C | ASTME831 | 1.3E-04 cm/cm/°C |