density | ASTM D792 | 0.924 g/cm³ | |
melt mass-flow rate | 190℃/2.16Kg | ASTM D1238 | 0.60 g/10min |
optical performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Haze ratio | ASTM D1003 | 9.0 % | |
gloss | ASTM2457 | 60 % | |
ASTM2457 | 84 % |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Secant modulus | ASTM D882 | 140 MPa | |
ASTM D882 | 170 MPa | ||
tensile strength | 断裂 | ASTM D882 | 25.0 MPa |
断裂 | ASTM D882 | 23.0 MPa | |
elongation at break | ASTM D882 | 350 % | |
ASTM D882 | 700 % | ||
Elmendorf tear strength | ASTM D1922 | 310 g | |
ASTM D1922 | 250 g | ||
ASTM D1922 | 6.20 g/micron | ||
ASTM D1922 | 5.00 g/micron |
Other performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Barrel Temperature | 180-185 °C | ||
Dart impact | ASTM D1709 | 3.40 g/micron | |
ASTM D1709 | 170 g | ||
Nozzle opening size | 0.100 cm | ||
Inflation ratio (BUR) | 2.0-3.0 | ||
temperature range | 150-185 °C |