physical property | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
melt mass-flow rate | 224°C/8.7kg | ASTM D1238 | 24 g/10min |
Shrinkage rate | MD | ASTM D955 | 0.0-0.60 % |
Shrinkage rate | TD | ASTM D955 | 0.50-0.70 % |
hardness | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Shore hardness | 邵氏A | ASTM D2240 | 88 |
Shore hardness | 邵氏D | ASTM D2240 | 48 |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Taber abraser | 1000g,H-22转轮 | ASTM D1044 | 5.00 mg |
elastomer | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
tear strength | 3.20mm | ASTM D624 | 82.3 kN/m |
compression set | 25°C,22hr | ASTM D395B | 25 % |
compression set | 70°C,22hr | ASTM D395B | 80 % |
tensile strength | 50%应变,3.20mm | ASTM D412 | 5.50 Mpa |
tensile strength | 100%应变,3.20mm | ASTM D412 | 6.90 Mpa |
tensile strength | 300%应变,3.20mm | ASTM D412 | 12.1 Mpa |
tensile strength | 断裂,3.20mm | ASTM D412 | 32.0 Mpa |
elongation | 断裂,3.20mm | ASTM D412 | 560 % |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Glass Transition Temperature | | DSC | -38.0 °C |
vicat | | ASTM D15252 | 67.2 °C |
Linear coefficient of thermal expansion | MD | ASTM D696 | 1.7E-04 cm/cm/°C |