برگه داده فنی
hardness | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
IRHD hardness | | ASTMD1415 | 75 |
Supplementary Information | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Low temperature resistance | Non-brittlefor3minutes | ASTM D2137 | -5 °C |
Low temperature resistance | TR10 | ISO 2921 | 2 °C |
Low temperature resistance | Non-brittlefor3minutes | ISO R812 | -5 °C |
Low temperature resistance | TR10 | ASTM D1329 | 2 °C |
elastomer | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
tensile strength | Yield | ASTMD412 | 21.4 MPa |
elongation | Break | ASTMD412 | 180 % |
compression set | 200°C,24hr | ASTM D395B | 28 % |
compression set | 200°C,24hr2 | ISO 815 | 28 % |
aging | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Change rate of tensile strength in air | 200°C,72hr | ASTMD412 | -6.0 % |
Change rate of ultimate elongation in air | 200°C,72hr | ASTMD412 | 18 % |
Change rate of IRHD hardness in the air | 200°C,72hr | ASTMD573 | 1.0 |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
maximum service temperature | Intermittent,shortterm | | 290 °C |
maximum service temperature | -- | | 250 °C |