plas
ورود

ASA Luran®S  777K UV BASF GERMANY

47

برگه داده فنی

impact performanceشرایط آزمونروش آزموننتیجه آزمون
Charpy Notched Impact Strength-30°CISO 1794.0 kJ/m²
Charpy Notched Impact Strength23°CISO 17917 kJ/m²
Impact strength of cantilever beam gap-30°CISO 180/A4.0 kJ/m²
Impact strength of cantilever beam gap23°CISO 180/A14 kJ/m²
mechanical propertiesشرایط آزمونروش آزموننتیجه آزمون
Tensile modulusISO 527-22300 Mpa
tensile strengthYield,23°CISO 527-248.0 Mpa
Tensile strainYield,23°CISO 527-23.3 %
Tensile creep modulus1hrISO 899-11850 Mpa
Tensile creep modulus1000hrISO 899-11400 Mpa
bending strengthISO 17870.0 Mpa
thermal performanceشرایط آزمونروش آزموننتیجه آزمون
Hot deformation temperature0.45MPa,AnnealedISO 75-2/B101 °C
Hot deformation temperature1.8MPa,AnnealedISO 75-2/A97.0 °C
Vicat softening temperature--ISO 306/A50105 °C
Vicat softening temperature--ISO 306/B5097.0 °C
Linear coefficient of thermal expansionMDISO 11359-28.0E-5to1.1E-4 cm/cm/°C
thermal conductivityDIN 526120.17 W/m/K
Physical propertiesشرایط آزمونروش آزموننتیجه آزمون
densityISO 11831.07 g/cm³
Melt Volume Flow Rate (MVR)220°C/10.0kgISO 113315.0 cm3/10min
Shrinkage rateISO 294-40.50-0.90 %
Water absorption rateSaturation,23°CISO 621.7 %
Water absorption rateEquilibrium,23°C,50%RHISO 620.35 %
Electrical performanceشرایط آزمونروش آزموننتیجه آزمون
Surface resistivityIEC 600931E+13 ohms
Volume resistivityIEC 600931E+14 ohms·cm
Dielectric constant100HzIEC 602503.70
Dissipation factor100HzIEC 602500.011
Dissipation factor1MHzIEC 602500.024
hardnessشرایط آزمونروش آزموننتیجه آزمون
Ball Pressure TestISO 2039-180.0 Mpa
filmشرایط آزمونروش آزموننتیجه آزمون
elongationBreakISO 527-39.0 %
نکات مهم: Plas.com داده‌های برگه فنی را از تولیدکنندگان مواد جمع‌آوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت داده‌ها انجام می‌دهد، اما هیچ مسئولیتی در قبال داده‌ها ندارد. اکیداً توصیه می‌شود که صحت داده‌ها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.