physical property شرایط آزمونروش آزموننتیجه آزمون
ash content--ISO 345141 %
ash content--ASTM D563041 %
densityASTM D7921.61 g/cm³
densityISO 11831.61 g/cm³
melt mass-flow rate300°C/1.2kgASTM D123820 g/10min
melt mass-flow rate300°C/1.2kgISO 113320 g/10min
optical performance شرایط آزمونروش آزموننتیجه آزمون
Yellowness Index--ASTM D19254.0 YI
Yellowness Index3.20mmASTM D19254.0 YI
Mechanical propertiesشرایط آزمونروش آزموننتیجه آزمون
elongationBreakASTM D6381.5 %
Tensile strainBreakISO 527-2/51.5 %
tensile strength YieldASTM D63861.0 MPa
tensile strength YieldISO 527-2/5620 MPa
Flexural modulusASTM D7907600 MPa
Flexural modulusISO 17877000 MPa
bending strengthASTM D79078.0 MPa
bending strengthISO 178800 MPa
Impact resistanceشرایط آزمونروش آزموننتیجه آزمون
Impact strength of cantilever beam gap23°C,6.35mmASTM D256150 J/m
Suspended wall beam without notch impact strength-5°CISO 180/1U16 kJ/m²
Charpy Notched Impact Strength23°CISO 179/1eA2.8 kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU13 kJ/m²
Impact strength of cantilever beam gap23°C,3.18mmASTM D25629 J/m
Impact strength of cantilever beam gap23°C,6.35mmASTM D25629 J/m
Impact strength of cantilever beam gap23°CISO 180/1A3.0 kJ/m²
Impact strength of cantilever beam gap23°C,3.18mmASTM D256160 J/m
Thermal performanceشرایط آزمونروش آزموننتیجه آزمون
Heat distortion temperature1.8MPa,未退火,6.40mm,HDTASTM D648250 °C
Heat distortion temperature1.8MPa,Unannealed,4.00mm,HDTISO 75-2/A250 °C