برگه داده فنی
physical property | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
density | | ASTM D792 | 1.04 g/cm³ |
Shrinkage rate | MD | ASTM D995 | 0.2 % |
Shrinkage rate | TD | ASTM D995 | 0.6 % |
Water absorption rate | (23°C,24hr) | ASTM D570 | 0.1 % |
hardness | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Rockwell hardness | | ASTM D785 | 84 R |
optical performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
refractive index | | ASTM542 | 1.57 |
Haze ratio | | ASTM D1003 | 2 % |
transmissivity | | ASTM D1003 | >=90 |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
tensile strength | 屈服,23°C | ASTM D638 | 26.2 MPa |
elongation at break | 23°C | ASTM D638 | 40 % |
Tensile modulus | 23°C | ASTM D638 | 2140 MPa |
bending strength | 23°C | ASTM D790 | 48.3 MPa |
Flexural modulus | 23°C | ASTM D790 | 1930 MPa |
Impact strength of cantilever beam gap | 23°C | ASTM D256 | 160 J/m |
Impact strength of cantilever beam gap | 加德纳冲击 | ASTM D5420 | 16.9 J |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
vicat | 1.02kg | ASTM1525 | 98.9 °C |
vicat | Melting Temperature | ASTM D4591 | 204-238 °C |
vicat | 最大使用温度 | | 249 °C |