PEI Generic PEI - Carbon Fiber Generic
ویژگیها:
Filler carbon fiber reinforced material
توصیف محصول
گواهینامهها(0)
جدول خواص
توصیف محصول
| ویژگیها: | Filler | carbon fiber reinforced material |
گواهینامهها
No Data...
برگه داده فنی
| impact performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 42to70 | J/m |
| 23°C | ISO 180 | 5.3to7.1 | kJ/m² | |
| Suspended wall beam without notch impact strength | 23°C | ASTM D256 | 270to660 | J/m |
| 23°C | ISO 180 | 18to45 | kJ/m² | |
| Dart impact | 23°C | ASTM D3763 | 6.21to10.5 | J |
| mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| bending strength | Break,23°C | ASTM D790 | 193to278 | MPa |
| Friction coefficient | ASTM D1894 | 0.39to0.52 | ||
| elongation | Break,23°C | ASTM D638 | 0.94to5.1 | % |
| Yield,23°C | ISO 527-2 | 0.95to2.0 | % | |
| Yield,23°C | ASTM D638 | 1.5to5.1 | % | |
| tensile strength | 23°C | ASTM D638 | 137to236 | MPa |
| Break,23°C | ISO 527-2 | 157to248 | MPa | |
| Break,23°C | ASTM D638 | 130to273 | MPa | |
| Tensile modulus | 23°C | ISO 527-2 | 11700to35700 | MPa |
| 23°C | ASTM D638 | 7860to31200 | MPa | |
| bending strength | 23°C | ISO 178 | 206to390 | MPa |
| 23°C | ASTM D790 | 193to295 | MPa | |
| Bending modulus | 23°C | ISO 178 | 12000to30600 | MPa |
| 23°C | ASTM D790 | 5960to26600 | MPa | |
| elongation | Break,23°C | ISO 527-2 | 0.90to2.1 | % |
| thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 2.6E-5到6.0E-5 | cm/cm/°C |
| TD | ASTME831 | 2.6E-5到4.0E-5 | cm/cm/°C | |
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 210to214 | °C |
| 1.8MPa,Unannealed | ASTM D648 | 207to214 | °C | |
| 1.8MPa,Unannealed | ISO 75-2/A | 200to214 | °C | |
| Linear coefficient of thermal expansion | MD | ASTME831 | 2.7E-6到1.9E-5 | cm/cm/°C |
| MD | ISO 11359-2 | 3.0E-6到2.7E-5 | cm/cm/°C | |
| Physical properties | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.20to0.29 | % |
| 23°C,24hr | ASTM D570 | 0.11to0.20 | % | |
| Shrinkage rate | TD:23°C | ASTM D955 | 0.39to0.41 | % |
| MD:23°C | ASTM D955 | 2.0E-3-0.25 | % | |
| density | 23°C | ISO 1183 | 1.34to1.50 | g/cm³ |
| -- | ASTM D792 | 1.30to1.48 | g/cm³ | |
| Shrinkage rate | 23°C | ISO 294-4 | 0.096to0.41 | % |
| Electrical performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Volume resistivity | 23°C | ASTM D257 | 1.0E+2到1.3E+10 | ohms·cm |
| Surface resistivity | ASTM D257 | 4.5E+2到1.3E+10 | ohms |
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.