physical property | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
density | ASTM D792/ISO 1183 | 1.04 | |
Shrinkage rate | ASTM D955 | 0.60% % | |
melt mass-flow rate | ASTM D1238/ISO 1133 | 36 g/10min |
optical performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Haze ratio | ISO 14782 | 0.50% % | |
transmittance | ASTM D1003/ISO 13468 | 90% % | |
refractive index | ASTM D542/ISO 489 | 1.540 |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Charpy Notched Impact Strength | ASTM D256/ISO 179 | 10 kg·cm/cm(J/M)ft·lb/in | |
Impact strength of cantilever beam gap | ASTM D256/ISO 179 | 25 kg·cm/cm(J/M)ft·lb/in | |
elongation at break | ASTM D638/ISO 527 | 3.0% kg/cm²(MPa)[Lb/in²] | |
Flexural modulus | ASTM D790/ISO 178 | 3200 kg/cm²(MPa)[Lb/in²] | |
bending strength | ASTM D790/ISO 178 | 100 kg/cm²(MPa)[Lb/in²] | |
tensile strength | ASTM D638/ISO 527 | 60 kg/cm²(MPa)[Lb/in²] |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Heat distortion temperature | HDT | ASTM D648/ISO 75 | 135 ℃(℉) |
HDT | ASTM D648/ISO 75 | 125 ℃(℉) |