PBT Generic ABS+PBT - Glass Fiber Generic
ویژگیها:
Filler glass fiber reinforced material
توصیف محصول
گواهینامهها(0)
جدول خواص
توصیف محصول
| ویژگیها: | Filler | glass fiber reinforced material |
گواهینامهها
No Data...
برگه داده فنی
| impact performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179 | 5.9to8.2 | kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 56to83 | J/m |
| mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| bending strength | 23°C | ISO 178 | 114to171 | MPa |
| 23°C | ASTM D790 | 86.1to190 | MPa | |
| Bending modulus | 23°C | ISO 178 | 3800to9770 | MPa |
| 23°C | ASTM D790 | 3180to10300 | MPa | |
| tensile strength | Break,23°C | ASTM D638 | 77.5to112 | MPa |
| Yield,23°C | ISO 527-2 | 78.8to120 | MPa | |
| elongation | Break,23°C | ISO 527-2 | 2.5to3.5 | % |
| tensile strength | 23°C | ASTM D638 | 77.7to105 | MPa |
| elongation | Break,23°C | ASTM D638 | 1.5to4.4 | % |
| tensile strength | Yield,23°C | ASTM D638 | 67.1to123 | MPa |
| thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 7.9E-5到1.0E-4 | cm/cm/°C |
| MD | ISO 11359-2 | 2.0E-5到4.0E-5 | cm/cm/°C | |
| MD | ASTM D696 | 2.8E-5到6.6E-5 | cm/cm/°C | |
| Vicat softening temperature | ISO 306 | 100to218 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 104to191 | °C |
| 1.8MPa,Unannealed | ASTM D648 | 104to202 | °C | |
| 0.45MPa,Unannealed | ISO 75-2/B | 196to220 | °C | |
| 0.45MPa,Unannealed | ASTM D648 | 198to211 | °C | |
| RTI Elec | UL 746 | 59.0to140 | °C | |
| RTI Imp | UL 746 | 58.8to100 | °C | |
| RTI | UL 746 | 60.0to130 | °C | |
| Physical properties | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.15 | % |
| 23°C,24hr | ASTM D570 | 0.12to0.15 | % | |
| Shrinkage rate | MD:23°C | ASTM D955 | 0.20to0.67 | % |
| melt mass-flow rate | 250°C/5.0kg | ASTM D1238 | 14to40 | g/10min |
| density | 23°C | ISO 1183 | 1.28to1.61 | g/cm³ |
| -- | ASTM D792 | 1.23to1.55 | g/cm³ | |
| Electrical performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 | ||
| Arc resistance | ASTM D495 | 69.0to85.5 | sec | |
| Dielectric strength | 23°C | ASTM D149 | 18to35 | kV/mm |
| Volume resistivity | 23°C | IEC 60093 | 1.0E+15到2.5E+17 | ohms·cm |
| 23°C | ASTM D257 | 1.0E+15到1.0E+17 | ohms·cm | |
| High arc combustion index | HAI | UL 746 | PLC 1 | |
| High voltage arc tracing rate | HVTR | UL 746 | PLC 4 | mm/min |
| Hot wire ignition | HWI | UL 746 | PLC 2 | sec |
| hardness | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Rockwell hardness | 23°C | ASTM D785 | 114to120 |