برگه داده فنی
physical property | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
density | | ASTM D792 | 0.918 g/cm³ |
Apparent density | | ASTM D1895 | 530 kg/m³ |
melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 1.0 g/10min |
optical performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
gloss | 45°,25.0µm,吹塑薄膜 | ASTM D2457 | 55 |
Haze ratio | 25.0µm,吹塑薄膜 | ASTM D1003 | 14 % |
Supplementary Information | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
PunctureEnergy | 25.0µm | 内部方法 | 700 J/cm |
film | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
film thickness | | | 25 µm |
Secant modulus | 1%正割,MD:25µm,吹塑薄膜 | ASTM D882 | 193 MPa |
Secant modulus | 1%正割,TD:25µm,吹塑薄膜 | ASTM D882 | 221 MPa |
tensile strength | MD:断裂,25µm,吹塑薄膜 | ASTM D882 | 34.0 MPa |
tensile strength | TD:断裂,25µm,吹塑薄膜 | ASTM D882 | 26.0 MPa |
Dart impact | Blown Film | ASTM D1709A | 110 g |
Elmendorf tear strength | MD:25.0µm | ASTM D1922 | 35.0 kN/m |
Elmendorf tear strength | TD:25.0µm | ASTM D1922 | 135.0 kN/m |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
melting temperature | | 内部方法 | 124 °C |
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.