برگه داده فنی
other | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
notes | | | 连接器 |
characteristic | | | 耐高温270度 |
Color | | | 本色 |
purpose | | | 连接器 |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Charpy Notched Impact Strength | | ASTM D256/ISO 179 | 110 kg·cm/cm(J/M)ft·lb/in |
Impact strength of cantilever beam gap | | ASTM D256/ISO 179 | 110 kg·cm/cm(J/M)ft·lb/in |
elongation at break | | ASTM D638/ISO 527 | 4.0% % |
tensile strength | | ASTM D638/ISO 527 | 712 kg/cm²(MPa)[Lb/in²] |
Rockwell hardness | | ASTM D785 | 30 |
Flexural modulus | | ASTM D790/ISO 178 | 112 kg/cm²(MPa)[Lb/in²] |
bending strength | | ASTM D790/ISO 178 | 205 kg/cm²(MPa)[Lb/in²] |
Electrical performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
dielectric constant | | ASTM D150/IEC 60250 | 30 |
Physical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
density | | ASTM D792/ISO 1183 | 1.37 |
Shrinkage rate | | ASTM D955 | 0.2 % |
melt mass-flow rate | | ASTM D1238/ISO 1133 | 45 g/10min |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Combustibility (rate) | | UL 94 | HB |
Heat distortion temperature | HDT | ASTM D648/ISO 75 | 270 ℃(℉) |