برگه داده فنی
other | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Color | | | 本色、黑色 |
processability | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Dry conditions | | | 95℃.4-6小时 |
process temperature | | | 260 °C |
process temperature | | | 280 °C |
process temperature | | | 270 °C |
process temperature | | | 290 °C |
Temperature | | | 85 °C |
pressure | | | 90-120 Mpa |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Charpy Notched Impact Strength | | ASTM D256/ISO 179 | 12 kg·cm/cm(J/M)ft·lb/in |
Charpy Notched Impact Strength | | ASTM D256/ISO 179 | 60 kg·cm/cm(J/M)ft·lb/in |
elongation at break | | ASTM D638/ISO 527 | 2.5 % |
tensile strength | | ASTM D638/ISO 527 | 150 kg/cm²(MPa)[Lb/in²] |
Flexural modulus | | ASTM D790/ISO 178 | 8500 kg·cm/cm(J/M)ft·lb/in |
bending strength | | ASTM D790/ISO 178 | 240 kg·cm/cm(J/M)ft·lb/in |
Electrical performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
dielectric constant | | ASTM D150/IEC 60250 | 3.4 |
Volume resistivity | | ASTM D257/IEC 60093 | 1*10^14 Ω.cm |
Physical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
density | | ASTM D792/ISO 1183 | 1.62 |
Shrinkage rate | | ASTM D955 | 0.4-0.7 % |
Water absorption rate | | ASTM D570/ISO 62 | 0.82 % |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Heat distortion temperature | HDT | ASTM D648/ISO 75 | 240 ℃(℉) |