برگه داده فنی
شرایط آزمون | روش آزمون | نتیجه آزمون | |
---|---|---|---|
elongation | Break | ASTM D882 | 150 % |
Elmendorf tear strength | MD | ASTM D1922 | 15 g |
Continuous use temperature | ASTM D794 | 218to260 °C | |
melting temperature | 302to310 °C | ||
Surface Resistivity | ASTM D257 | 1E+15 ohms | |
Volume resistivity | ASTM D257 | 1E+16 ohms·cm | |
dielectric strength | ASTM D149 | 120 kV/mm | |
dielectric constant | 1kHz | ASTM D150 | 2.15 |
tensile strength | Break | ASTM D882 | 27.6 MPa |
Dissipation Factor | 1kHz | ASTM D150 | 5E-04 |
UL flame retardant rating | UL 94 | V-0 | |
refractive index | ASTM D542 | 1.350 | |
Haze ratio | ASTM D1003 | 4.0 % | |
density | ASTM D792 | 2.14 g/cm³ | |
Water absorption rate | 24hr | ASTM D570 | 0.010 % |
coefficient of friction | Itself - Static | ASTM D1894 | 0.045 |
film thickness | 25 µm | ||
tensile strength | Yield | ASTM D882 | 13.8 MPa |