برگه داده فنی
Basic performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
relative viscosity | GB T1632-93 | 2.45 | |
Monomer content | ≤0.5 % | ||
density | GB 1033-86 | 1.14 g/cm³ | |
Shrinkage rate | 1.3 % | ||
water content | ≤0.05 % |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Tensile modulus | ASTM D-638 | 2142.0 Mpa | |
bending strength | ASTM D-790 | 112.8 Mpa | |
elongation | 断裂 | ASTM D-638 | 71.0 % |
Impact strength of cantilever beam gap | ASTM D-256 | 10.0 kJ/m² | |
tensile strength | ASTM D 638 | 70.5 Mpa | |
Flexural modulus | ASTM D-790 | 1971.9 Mpa | |
Shore hardness | ASTM D-785 | 17.4 Kgf/mm2 |
Electrical performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Dielectric loss | 正切 | ASTM D-150 | 0.030 MHz |
dielectric constant | ASTM D-150 | 3.2 MHz |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Heat distortion temperature | 1.82MPa,HDT | ASTM D-648 | 54 °C |
UL flame retardant rating | UL 94 | V-2 | |
melt mass-flow rate | ASTM D-1238 | 26.0 g/10min |