    Filler glass fiber reinforced material
  • مقایسه

برگه داده فنی

optical performanceشرایط آزمونروش آزموننتیجه آزمون
Huangdu Index3.20mmASTM D19253.0 YI
Huangdu Index--ASTM D19253.0 YI
impact performanceشرایط آزمونروش آزموننتیجه آزمون
Charpy Notched Impact Strength23°CISO 179/1eA2.0 kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU25 kJ/m²
Impact strength of cantilever beam gap23°C,3.18mmASTM D25629 J/m
Impact strength of cantilever beam gap23°C,6.35mmASTM D25629 J/m
Impact strength of cantilever beam gap23°CISO 180/1A2.0 kJ/m²
Impact strength of cantilever beam gap23°C,3.18mmASTM D256300 J/m
Impact strength of cantilever beam gap23°C,6.35mmASTM D256290 J/m
Suspended wall beam without notch impact strength-5°CISO 180/1U30 kJ/m²
mechanical propertiesشرایط آزمونروش آزموننتیجه آزمون
bending strengthASTM D79094.0 MPa
bending strengthISO 17888.0 MPa
tensile strengthYieldASTM D63866.0 MPa
tensile strengthYieldISO 527-2/558.0 MPa
elongationBreakASTM D6382.0 %
Tensile strainBreakISO 527-2/52.0 %
Bending modulusASTM D7905500 MPa
Bending modulusISO 1785400 MPa
thermal performanceشرایط آزمونروش آزموننتیجه آزمون
Hot deformation temperature1.8MPa,Unannealed,6.40mmASTM D648245 °C
Hot deformation temperature1.8MPa,Unannealed,4.00mmISO 75-2/A245 °C
Physical propertiesشرایط آزمونروش آزموننتیجه آزمون
melt mass-flow rate300°C/2.16kgASTM D123860 g/10min
melt mass-flow rate300°C/2.16kgISO 113360 g/10min
densityASTM D7921.53 g/cm³
densityISO 11831.53 g/cm³