برگه داده فنی
physical property | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Shrinkage rate | ASTM D-955 | 0.4-0.8 % | |
density | ASTM D-792 | 1.18 | |
fire retardancy | UL 94 | HB CLASS | |
refractive index | ASTM D-542 | 1.49 | |
transmittance | ASTM D-1003 | 93 % |
Basic performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Water absorption rate | 浸水24hrs后増重 | ASTM D-570 | 0.3 % |
melt mass-flow rate | ASTM D-1238 | 2 g/min |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
bending strength | 横夸比=16 | ASTM D-790 | 1460(143) Kgf/cm |
Flexural modulus | ASTM D-790 | 34000 Kgf/cm | |
tensile strength | 初级应变速率0.1cm/cm/min | ASTM D-638 | 767(75) Kgf/cm |
Rockwell hardness | ASTM D-758(M级) | 99 | |
Impact strength of cantilever beam gap | 落锤(15.2*15.2*0.3cm)重1.4kg 半径0.64cm | ASTM D-256 | 14(1.6) kg-cm(J) |
Lzod 研磨缺口 | ASTM D-256 | 1.5(14.7) kgf-cm/cm(J/m) |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
vicat | 50℃/hr,1kg | ASTM D-1525 | 235 F |
Temperature range for use | 与残余应力大小有关 | 85-105 | |
vicat | 未退火 | ASTM D-1525 | 113 °C |
Heat distortion temperature | HDT | ASTM D-648 | 103 °C |