PA6 TAROMID B 280 G5 Taro Plast S.p.A.
ویژگیها:
Filler glass fiber reinforced material 25% filler by weight
توصیف محصول
گواهینامهها(0)
جدول خواص
توصیف محصول
| ویژگیها: | Filler | glass fiber reinforced material | 25% | filler by weight |
گواهینامهها
No Data...
برگه داده فنی
| impact performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179 | 7.5 | kJ/m² |
| Impact strength of cantilever beam gap | 23°C,3.20mm | ASTMD256 | 100 | J/m |
| flammability | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Extreme Oxygen Index | ASTM D2863 | 24 | % | |
| Hot filament ignition temperature | 2.0mm | IEC 60695-2-13 | 750 | °C |
| UL flame retardant rating | 1.6mm | UL 94 | HB | |
| mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| bending strength | Break | ASTM D790 | 240 | MPa |
| -- | ISO 178 | 240 | MPa | |
| Bending modulus | ASTMD790 | 8000 | MPa | |
| elongation | Break | ASTMD638 | 3.5 | % |
| tensile strength | Break | ASTMD638 | 160 | MPa |
| Tensile modulus | ASTMD638 | 8300 | MPa | |
| thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Continuous use temperature | --5 | IEC 60216 | 140 | °C |
| Linear coefficient of thermal expansion | MD:-30to30°C | ASTM D696 | 3.5E-05 | cm/cm/°C |
| Melting temperature | ASTMD211 | 222 | °C | |
| Vicat softening temperature | ISO 306/B50 | 210 | °C | |
| Continuous use temperature | --6 | IEC 60216 | 180 | °C |
| Hot deformation temperature | 1.8MPa,Unannealed | ASTMD648 | 200 | °C |
| Continuous use temperature | --3 | IEC 60216 | 100 | °C |
| --4 | IEC 60216 | 130 | °C | |
| Physical properties | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Water absorption rate | Saturation,23°C | ISO 62 | 6.5 | % |
| Saturation | ASTM D570 | 6.5 | % | |
| 23°C,24hr | ASTMD570 | 1.0 | % | |
| Shrinkage rate | TD | ASTM D955 | 0.60to0.80 | % |
| MD | ASTM D955 | 0.30to0.40 | % | |
| melt mass-flow rate | 250°C/2.16kg | ASTMD1238 | 12 | g/10min |
| density | ASTMD792 | 1.30to1.32 | g/cm³ | |
| GranuleHumidity | Internal Method | <0.10 | % | |
| Electrical performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 1 | |
| Volume resistivity | ASTM D257 | 7E+15 | ohms·cm | |
| hardness | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Rockwell hardness | R-Scale | ASTM D785 | 120 |
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.