برگه داده فنی
physical property | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
density | -- | ASTM D792 | 1.28to1.36 g/cm³ |
density | 23°C | ISO 1183 | 1.29to1.30 g/cm³ |
melt mass-flow rate | 365°C/5.0kg | ASTM D1238 | 7.0to37 g/10min |
Shrinkage rate | MD:23°C | ASTM D955 | 0.70to0.71 % |
Shrinkage rate | 23°C | ISO 294-4 | 0.70to1.0 % |
Water absorption rate | 23°C,24hr | ASTM D570 | 0.36to0.38 % |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Tensile modulus | 23°C | ASTM D638 | 2330to2360 MPa |
Tensile modulus | 23°C | ISO 527-2 | 2270to2800 MPa |
tensile strength | 23°C | ASTM D638 | 69.1to70.7 MPa |
elongation | 屈服,23°C | ASTM D638 | 7.0to90 % |
elongation | 断裂,23°C | ASTM D638 | 28to90 % |
Flexural modulus | 23°C | ASTM D790 | 2340to2410 MPa |
bending strength | 23°C | ASTM D790 | 89.3to100 MPa |
Impact resistance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Impact strength of cantilever beam gap | 23°C | ASTM D256 | 680to690 J/m |
Electrical performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
dielectric constant | 23°C | ASTM D150 | 3.32to3.54 |
Volume resistivity | 23°C | ASTM D257 | 1.0E+12到9.0E+15 ohms·cm |
dielectric strength | 23°C | ASTM D149 | 12to200 kV/mm |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 206to209 °C |
Linear coefficient of thermal expansion | MD:-- | ASTM D696 | 5.5E-5到7.2E-5 cm/cm/°C |
Linear coefficient of thermal expansion | MD:-- | ISO 11359-2 | 5.5E-05 cm/cm/°C |
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.