optical performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Haze ratio | | ASTM D-1003 | 4.5 % |
gloss | 45℃ | ASTM D-523 | 78 |
Basic performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Vinyl acetate content | | | 9.0 % |
melt mass-flow rate | | ASTM D-1238 | 2.0 g/10min |
density | | ASTM D-1505 | 0.929 g/cm3 |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
tensile strength | | ASTM D-638 | 7 MPa |
elongation at break | | ASTM D-638 | 12 MPa |
elongation at break | | ASTM D-638 | 1200 % |
Shore hardness | | ASTM D-2240 | 45 |
Dart impact | | ASTM D-1709 | 330 g |
elongation at break | TD | ASTM D-882 | 475 % |
elongation at break | MD | ASTM D-882 | 325 % |
tensile strength | TD,断裂 | ASTM D-882 | 19 MPa |
tensile strength | MD,断裂 | ASTM D-882 | 23 MPa |
Other performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Melt Temperature | | ASTM D-1525 | 182-193 ℃ |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
vicat | | ASTM D-1525 | 76 ℃ |