مقایسه مواد
افزودن مدل برای مقایسه
انتخاب محصولات برای مقایسه (1/4)
برجسته کردن تفاوت ها
مخفی کردن موارد مشابه
نام محصول / تولیدکننده / مدل
درجه
گواهینامهها
قیمت مرجع
| flammability | شرایط آزمون | روش آزمون | DUPONT USA/ST820 NC010 |
|---|---|---|---|
| UL flame retardant rating | 0.8mm | UL 94 | HB |
| Extreme Oxygen Index | ISO 4589-2 | 19 % | |
| Fogging-G-value | condensate | ISO 6452 | 1E-04 g |
| Burning rate | 1.00mm | ISO 3795 | 38 mm/min |
| UL flame retardant rating | 0.8mm | IEC 60695-11-10,-20 | HB |
| FMVSS flammability | FMVSS302 | B | |
| mechanical properties | شرایط آزمون | روش آزمون | DUPONT USA/ST820 NC010 |
| Impact strength of cantilever beam gap | 23℃ | ASTM D256 | No Break J/m |
| bending strength | ISO 178 | 50.0 Mpa | |
| Elongation at Break | 23℃ | ASTM D638 | 150 % |
| Tensile modulus | ISO 527-2 | 1700 Mpa | |
| bending strength | ASTM D790/ISO 178 | 50 kg/cm²(MPa)[Lb/in²] | |
| Nominal tensile fracture strain | ISO 527-2 | >50 % | |
| Bending modulus | ISO 178 | 1550 Mpa | |
| bending strength | 23℃ | ASTM D638 | 53 MPa |
| Bending modulus | ASTM D790/ISO 178 | 1550 kg/cm²(MPa)[Lb/in²] | |
| 23℃ | ASTM D790 | 1680 MPa | |
| Suspended wall beam without notch impact strength | 23℃ | ASTM D256 | No Break J/m |
| Tensile modulus | 23℃ | ASTM D638 | 1600 MPa |
| Tensile strain | Yield | ISO 527-2 | 7.0 % |
| Tensile modulus | ASTM D638/ISO 527 | 1700 kg/cm²(MPa)[Lb/in²] | |
| Suspended wall beam without notch impact strength | -40℃ | ASTM D256 | No Break J/m |
| compressive strength | 23℃ | ASTM D695 | 43 MPa |
| Elongation at Break | ASTM D638/ISO 527 | 150 % | |
| tensile strength | Yield | ISO 527-2 | 38.0 Mpa |
| Impact strength of cantilever beam gap | -40℃ | ASTM D256 | 117 J/m |
| ASTM D256 | 117 J/m | ||
| tensile strength | 23℃ | ASTM D638 | 37 MPa |
| other | شرایط آزمون | روش آزمون | DUPONT USA/ST820 NC010 |
| characteristic | 无筋.超级坚固.注射成型 | ||
| Physical properties | شرایط آزمون | روش آزمون | DUPONT USA/ST820 NC010 |
| Shrinkage rate | MD | ISO 294-4 | 1.9 % |
| ASTM D955 | 1.8 % | ||
| Water absorption rate | Saturation,23°C,2.00mm | ISO 62 | 0.31 % |
| Top out temperature | 170 °C | ||
| Shrinkage rate | MD2 | ISO 294-4 | 2.5 % |
| SpecificHeatCapacity of Melt | 2100 J/kg/°C | ||
| Shrinkage rate | TD | ISO 294-4 | 1.8 % |
| density | ASTM D792/ISO 1183 | 1220 | |
| Water absorption rate | ASTM D570/ISO 62 | 0.12 % | |
| MediumDensity | 1.03 g/cm³ | ||
| Water absorption rate | Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 0.12 % |
| ThermalConductivityofMelt | 0.20 W/m/K | ||
| thermal performance | شرایط آزمون | روش آزمون | DUPONT USA/ST820 NC010 |
| Linear coefficient of thermal expansion | 平行Flow | ASTM E831 | 0.00019 cm/cm/℃ |
| Vicat softening temperature | ASTM D1525/ISO R306 | 216 ℃(℉) | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 50.0 °C |
| 264 psi,Unannealed | ASTM D648 | 47 ℃ | |
| 0.45MPa,Annealed | ISO 75-2/B | 145 °C | |
| Melting temperature | ISO 11357-3 | 225 °C | |
| Vicat softening temperature | ISO 306/B50 | 125 °C | |
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | 145 ℃(℉) |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 1.9E-04 cm/cm/°C |
| 垂直Flow | ASTM E831 | 0.00019 cm/cm/℃ | |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 100 °C |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1.9E-04 cm/cm/°C |
| Combustibility (rate) | UL 94 | HB(0.8mm) | |
| Melting temperature | 225 ℃(℉) | ||
| ℃ | 225 225 | ||
| Electrical performance | شرایط آزمون | روش آزمون | DUPONT USA/ST820 NC010 |
| Dissipation factor | 100Hz | IEC 60250 | 0.020 |
| Volume resistivity | IEC 60093 | >1.0E+15 ohms·cm | |
| Dissipation factor | 1MHz | IEC 60250 | 0.019 |
| Surface resistivity | IEC 60093 | 1E+15 ohms | |
| Dielectric strength | IEC 60243-1 | 27 KV/mm | |
| Surface resistivity | ASTM D257/IEC 60093 | 1.00E+15 Ω | |
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 | |
| Volume resistivity | ASTM D257/IEC 60093 | >1E13 Ω.cm | |
| impact performance | شرایط آزمون | روش آزمون | DUPONT USA/ST820 NC010 |
| Suspended wall beam without notch impact strength | -40°C | ISO 180/1U | 270 kJ/m² |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | NoBreak |
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | NoBreak |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | NoBreak |
| Suspended wall beam without notch impact strength | -30°C | ISO 180/1U | NoBreak |
| Other performance | شرایط آزمون | روش آزمون | DUPONT USA/ST820 NC010 |
| Extreme Oxygen Index | ASTM D2863 | 22 % | |
| hardness | شرایط آزمون | روش آزمون | DUPONT USA/ST820 NC010 |
| Rockwell hardness | R-Scale | ISO 2039-2 | 104 |