نام محصول / تولیدکننده / مدل
درجه
قیمت مرجع
| flame retardant performance | شرایط آزمون | روش آزمون | DUPONT KOREA/935 BK505 |
|---|---|---|---|
| Ignition temperature of heating wire | 3.00mm | IEC 60695-2-12 | 825 °C |
| Relative temperature of heating wire | 1.50mm | IEC 60695-2-13 | 800 °C |
| 0.75mm | IEC 60695-2-13 | 775 °C | |
| Ignition temperature of heating wire | 1.50mm | IEC 60695-2-12 | 775 °C |
| 0.75mm | IEC 60695-2-12 | 800 °C | |
| Relative temperature of heating wire | 3.00mm | IEC 60695-2-13 | 850 °C |
| UL flame retardant rating | UL -94 | HB 3.00mm | |
| mechanical properties | شرایط آزمون | روش آزمون | DUPONT KOREA/935 BK505 |
| tensile strength | 23°C | ISO 527-2 | 82.0 Mpa |
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 4.0 kJ/m² |
| bending strength | 23°C | ISO 178 | 132 Mpa |
| Elongation at Break | 23°C | ISO 527-2 | 2.0 % |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 25 kJ/m² |
| -40°C | ISO 179/1eU | 22 kJ/m² | |
| Bending modulus | 23°C | ISO 178 | 9300 Mpa |
| ISO 178 | 9300 Mpa | ||
| Tensile modulus | ISO 527-1 | 10200 Mpa | |
| Charpy Notched Impact Strength | -40°C | ISO 179/1eA | 4.0 kJ/m² |
| Tensile modulus | 23°C | ISO 527-2 | 10200 Mpa |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 5.5 kJ/m² |
| thermal performance | شرایط آزمون | روش آزمون | DUPONT KOREA/935 BK505 |
| Hot deformation temperature | 0.45MPaUnannealed | ISO 75-2/Bf | 240 °C |
| UL flame retardant rating | UL 94 | HB | |
| Hot deformation temperature | 1.80MPaAnnealed | ISO 75-2/Af | 200 °C |
| Physical properties | شرایط آزمون | روش آزمون | DUPONT KOREA/935 BK505 |
| Shrinkage rate | MD2.0mm | ISO 294-4 | 0.20 % |
| TD2.0mm | ISO 294-4 | 0.70 % | |
| Electrical performance | شرایط آزمون | روش آزمون | DUPONT KOREA/935 BK505 |
| Volume resistivity | IEC 60093 | 1E+14 Ω.cm | |
| Dielectric strength | IEC 60243-1 | 40 KV/mm |