نام محصول / تولیدکننده / مدل
درجه
قیمت مرجع
| optical performance | شرایط آزمون | روش آزمون | SABIC INNOVATIVE US/GLX143-NA9C029H |
|---|---|---|---|
| Refractive index | ISO 489 | 1.586 | |
| turbidity | 2540μm | ASTM D1003 | <0.80 % |
| transmissivity | 5000μm | ASTM D1003 | 87.0 % |
| 3000μm | ASTM D1003 | 89.0 % | |
| 6000μm | ASTM D1003 | 86.0 % | |
| 4000μm | ASTM D1003 | 88.0 % | |
| mechanical properties | شرایط آزمون | روش آزمون | SABIC INNOVATIVE US/GLX143-NA9C029H |
| bending strength | ISO 178 | 90.0 Mpa | |
| Tensile modulus | ISO 527-2/1 | 2350 Mpa | |
| tensile strength | Break | ISO 527-2/50 | 70.0 Mpa |
| Yield | ISO 527-2/50 | 65.0 Mpa | |
| Tensile strain | Break | ISO 527-2/50 | 120 % |
| Bending modulus | ISO 178 | 2300 Mpa | |
| Tensile strain | Yield | ISO 527-2/50 | 6.0 % |
| flammability | شرایط آزمون | روش آزمون | SABIC INNOVATIVE US/GLX143-NA9C029H |
| Burning wire flammability index | 1.00mm | IEC 60695-2-12 | 850 °C |
| Extreme Oxygen Index | ISO 4589-2 | 25 % | |
| thermal performance | شرایط آزمون | روش آزمون | SABIC INNOVATIVE US/GLX143-NA9C029H |
| 1.8MPa, unannealed, 64.0mm span of | ISO 75-2/Af | 124 °C | |
| RTI Elec | UL 746 | 130 °C | |
| Ball Pressure Test | 125°C | IEC 60695-10-2 | Pass |
| RTI Imp | UL 746 | 125 °C | |
| 1.8MPa, unannealed, 100mm span | ISO 75-2/Ae | 125 °C | |
| RTI | UL 746 | 125 °C | |
| thermal conductivity | ISO 8302 | 0.20 W/m/K | |
| Linear coefficient of thermal expansion | MD:23to80°C | ISO 11359-2 | 7E-05 cm/cm/°C |
| 0.45MPa, unannealed, 100mm span | ISO 75-2/Be | 136 °C | |
| Linear coefficient of thermal expansion | TD:23to80°C | ISO 11359-2 | 7E-05 cm/cm/°C |
| impact performance | شرایط آزمون | روش آزمون | SABIC INNOVATIVE US/GLX143-NA9C029H |
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 14 kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 70 kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 无断裂 |
| -30°C | ISO 179/1eU | 无断裂 | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 73 kJ/m² |
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 12 kJ/m² |
| Suspended wall beam without notch impact strength | -30°C | ISO 180/1U | 无断裂 |
| 23°C | ISO 180/1U | 无断裂 | |
| Physical properties | شرایط آزمون | روش آزمون | SABIC INNOVATIVE US/GLX143-NA9C029H |
| Shrinkage rate | MD1 | Internal Method | 0.50-0.70 % |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.15 % |
| Saturation,23°C | ISO 62 | 0.35 % | |
| Melt Volume Flow Rate (MVR) | 300°C/1.2kg | ISO 1133 | 12.0 cm3/10min |
| Electrical performance | شرایط آزمون | روش آزمون | SABIC INNOVATIVE US/GLX143-NA9C029H |
| Dissipation factor | 50Hz | IEC 60250 | 1E-03 |
| Relative permittivity | 50Hz | IEC 60250 | 2.70 |
| Dielectric strength | 3.20mm,in Oil | IEC 60243-1 | 17 KV/mm |
| 1.00mm11 | IEC 60243-1 | 15 KV/mm | |
| Dissipation factor | 1MHz | IEC 60250 | 0.010 |
| 60Hz | IEC 60250 | 1E-03 | |
| Relative permittivity | 1MHz | IEC 60250 | 2.70 |
| 60Hz | IEC 60250 | 2.70 |