برگه داده فنی impact performance شرایط آزمون روش آزمون نتیجه آزمون Suspended wall beam without notch impact strength 23°C ASTM D4812 640 J/m  Dart impact 23°C, Energy at Peak ASTM D3763 6.00 J  Dart impact 23°C, Total Energy ASTM D3763 8.00 J  
flammability شرایط آزمون روش آزمون نتیجه آزمون UL flame retardant rating 1.5 mm UL 94 HB  
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون tensile strength Break ASTM D638 110 Mpa  Bending modulus 50.0 mm Span ASTM D790 6890 Mpa  bending strength Break, 50.0 mm Span ASTM D790 189 Mpa  
injection شرایط آزمون روش آزمون نتیجه آزمون drying temperature 120 °C  drying time 3.0 to 4.0 hr  Suggested maximum moisture content 0.020 %  Suggested injection volume 40 to 80 %  Temperature at the rear of the barrel 240 to 255 °C  Temperature in the middle of the barrel 245 to 260 °C  Temperature at the front of the material cylinder 250 to 265 °C  Spray nozzle temperature 245 to 260 °C  Processing (melt) temperature 250 to 265 °C  Mold temperature 65 to 90 °C  Back pressure 0.300 to 0.700 Mpa  Screw speed 50 to 80 rpm  Exhaust hole depth 0.025 to 0.038 mm  
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Hot deformation temperature 0.45 MPa, Unannealed, 6.40 mm ASTM D648 215 °C  Hot deformation temperature 1.8 MPa, Unannealed, 6.40 mm ASTM D648 176 °C  Linear coefficient of thermal expansion -40 to 40°C,Flow ASTM E831 2.3E-5 cm/cm/°C  Linear coefficient of thermal expansion 60 to 138°C,Flow ASTM E831 1.6E-5 cm/cm/°C  RTI Elec UL 746 125 °C  RTI Imp UL 746 110 °C  RTI UL 746 125 °C  
Physical properties شرایط آزمون روش آزمون نتیجه آزمون Specific volume ASTM D792 0.660 cm³/g  Shrinkage rate Flow : 1.50 to 3.20 mm Internal Method 0.30 - 0.50 %  Shrinkage rate Flow : 3.20 to 4.60 mm Internal Method 0.50 - 0.80 %  Shrinkage rate Across FlowFlow : 1.50 to 3.20 mm Internal Method 0.40 - 0.60 %  Shrinkage rate Across FlowFlow : 3.20 to 4.60 mm Internal Method 0.60 - 0.90 %  Water absorption rate 24 hr ASTM D570 0.060 %  Outdoor applicability UL 746C f2  
Electrical performance شرایط آزمون روش آزمون نتیجه آزمون Volume resistivity ASTM D257 5.9E+16 ohms·cm  Dielectric strength 1.60 mm, in Oil ASTM D149 29 KV/mm  Dielectric strength 3.20 mm, in Air ASTM D149 24 KV/mm  Dielectric constant 100 Hz ASTM D150 3.60  Dielectric constant 1 MHz ASTM D150 3.60  Dissipation factor 100 Hz ASTM D150 1.4E-3  Dissipation factor 1 MHz ASTM D150 0.020  Arc resistance ASTM D495 PLC 6  Compared to the anti leakage trace index UL 746 PLC 4  High arc combustion index UL 746 PLC 3  High voltage arc tracing rate UL 746 PLC 2  Hot wire ignition UL 746 PLC 1  
hardness شرایط آزمون روش آزمون نتیجه آزمون Rockwell hardness R-Scale ASTM D785 119  