Impact strength of simply supported beam without notch
-30°C
ISO 179/1eU
75 kJ/m²
Impact strength of simply supported beam without notch
23°C
ISO 179/1eU
NoBreak
flammability
شرایط آزمون
روش آزمون
نتیجه آزمون
UL flame retardant rating
1.5mm
IEC 60695-11-10,-20
HB
UL flame retardant rating
3.0mm
IEC 60695-11-10,-20
HB
Burning wire flammability index
1.5mm
IEC 60695-2-12
675 °C
Burning wire flammability index
3.0mm
IEC 60695-2-12
675 °C
Hot filament ignition temperature
1.5mm
IEC 60695-2-13
700 °C
Hot filament ignition temperature
3.0mm
IEC 60695-2-13
700 °C
Burning rate
ISO 3795
30 mm/min
mechanical properties
شرایط آزمون
روش آزمون
نتیجه آزمون
Tensile modulus
ISO 527-2/1A/1
3100 Mpa
tensile strength
Yield
ISO 527-2/1A/50
51.0 Mpa
Tensile strain
Yield
ISO 527-2/1A/50
3.1 %
thermal performance
شرایط آزمون
روش آزمون
نتیجه آزمون
Hot deformation temperature
0.45MPa,Unannealed
ISO 75-2/Bf
96.0 °C
Hot deformation temperature
1.8MPa,Unannealed
ISO 75-2/Af
78.0 °C
Vicat softening temperature
--
ISO 306/A50
184 °C
Vicat softening temperature
--
ISO 306/B50
110 °C
Physical properties
شرایط آزمون
روش آزمون
نتیجه آزمون
Melt Volume Flow Rate (MVR)
250°C/5.0kg
ISO 1133
6.00 cm3/10min
hardness
شرایط آزمون
روش آزمون
نتیجه آزمون
Ball Pressure Test
H358/10
ISO 2039-1
101 Mpa
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.