برگه داده فنی مقایسهelastomer شرایط آزمون روش آزمون نتیجه آزمون Permanent compression deformation 70°C,22hr ISO 815 41 % Permanent compression deformation 100°C,70hr ASTM D395B 53 % Permanent compression deformation 70°C,22hr ASTM D395B 41 % elongation Break,23°C,Across Flow ISO 37 490 % elongation Break,23°C,Across Flow ASTM D412 490 % tensile strength Break,23°C ISO 37 6.60 Mpa tensile strength Break,23°C,横向Flow ASTM D412 6.60 Mpa Tensile stress 100%Strain,23°C,横向Flow ISO 37 2.30 Mpa Tensile stress 100%Strain,23°C,横向Flow ASTM D412 2.30 Mpa Permanent compression deformation 100°C,70hr ISO 815 53 %
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Brittle temperature ISO 812 -52.0 °C Brittle temperature ASTM D746 -52.0 °C
hardness شرایط آزمون روش آزمون نتیجه آزمون Shore hardness ShoreA,15Sec,23°C ISO 868 65
aging شرایط آزمون روش آزمون نتیجه آزمون Shore hardness ShoreA,100°C,1008hr ISO 188 2.0 Hardness change rate in the air ShoreA,100°C,1008hr ASTM D573 2.0 Elongation at Break 100°C,1008hr ASTM D573 -10 % Change rate of tensile strength in air 100°C,1008hr ISO 188 -3.0 % Change rate of tensile strength in air 100°C,1008hr ASTM D573 -3.0 %
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.