Impact strength of simply supported beam without notch
23℃
ISO 179
(14.5干态) kJ/m²
Charpy Notched Impact Strength
23℃
ISO 179
(100干态) kJ/m²
thermal performance
شرایط آزمون
روش آزمون
نتیجه آزمون
Hot deformation temperature
1.8MPa
ISO 75
245 °C
Vicat softening temperature
50℃/hr 50N
ISO 306
290 °C
Melting temperature
10℃/min
ISO 11357
295 °C
Glass transition temperature
10℃/min
ISO 11357
105 °C
Linear coefficient of thermal expansion
Flow
ISO 11359
1.5E-5 m/m/k
Linear coefficient of thermal expansion
垂直
ISO 11359
6.5E-5 m/m/k
Physical properties
شرایط آزمون
روش آزمون
نتیجه آزمون
density
ISO 1183
1430 g/cm³
Shrinkage rate
Flow
ISO 294
0.3 %
Shrinkage rate
垂直
ISO 294
1 %
Stickiness
ISO 307
130 ㎤/g
Electrical performance
شرایط آزمون
روش آزمون
نتیجه آزمون
Volume resistivity
IEC 62631
(1E+13干态)(1E+12湿态) Ω.m
Surface resistivity
IEC 62631-2-1
(1E+13湿态) Ω
Dielectric strength
IEC 60243
(33干态)(31湿态) KV/mm
Dielectric constant
1MHz
IEC 62631-2-1
(4.2干态)(4.4湿态)
Dissipation factor
1MHz
IEC 62631-2-1
(0.02干态)(0.03湿态)
Compared to the anti leakage trace index
IEC 60112
V