برگه داده فنی مقایسهimpact performance شرایط آزمون روش آزمون نتیجه آزمون Reverse notch impact 3.20 mm ASTM D256 400 J/m
flammability شرایط آزمون روش آزمون نتیجه آزمون UL flame retardant rating 0.41 mm UL 94 V-0 UL flame retardant rating 1.9 mm UL 94 5VA
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون Tensile modulus ASTM D638 4610 Mpa tensile strength Yield ASTM D638 114 Mpa tensile strength Break ASTM D638 115 Mpa elongation Break ASTM D638 6.0 % Bending modulus 100 mm Span ASTM D790 5240 Mpa bending strength Break, 100 mm Span ASTM D790 199 Mpa
injection شرایط آزمون روش آزمون نتیجه آزمون drying temperature 150 °C drying time 4.0 to 6.0 hr Suggested maximum moisture content 0.020 % Suggested injection volume 40 to 60 % Temperature at the rear of the barrel 330 to 400 °C Temperature in the middle of the barrel 340 to 400 °C Temperature at the front of the material cylinder 345 to 400 °C Spray nozzle temperature 345 to 400 °C Processing (melt) temperature 350 to 400 °C Mold temperature 135 to 165 °C Back pressure 0.300 to 0.700 Mpa Screw speed 40 to 70 rpm Exhaust hole depth 0.025 to 0.076 mm
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Hot deformation temperature 1.8 MPa, Unannealed, 6.40 mm ASTM D648 207 °C RTI Elec UL 746 170 °C RTI Imp UL 746 170 °C RTI UL 746 170 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون melt mass-flow rate 337°C/6.6 kg ASTM D1238 11 g/10 min
Electrical performance شرایط آزمون روش آزمون نتیجه آزمون Arc resistance ASTM D495 PLC 6 Compared to the anti leakage trace index UL 746 PLC 4 High arc combustion index UL 746 PLC 4 High voltage arc tracing rate UL 746 PLC 2 Hot wire ignition UL 746 PLC 1
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.