برگه داده فنی مقایسهother شرایط آزمون روش آزمون نتیجه آزمون characteristic 高光泽高耐热
Basic Performance شرایط آزمون روش آزمون نتیجه آزمون melt mass-flow rate 200℃,3.8kg ASTM D-1238 3.9 g/10min
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون Impact strength of cantilever beam gap 23°C ASTM D-256 28 kJ/m² elongation at yield 1/8",5mm/min ASTM D-638 2 % tensile strength 1/8",5mm/min,Break ASTM D-638 32 Mpa Elongation at Break 1/8",5mm/min ASTM D-638 25 % tensile strength Yield,1/8",5mm/min ASTM D-638 41 Mpa Elongation at Break ASTM D638/ISO 527 25 % Impact strength of cantilever beam gap ASTM D256/ISO 179 (28) kg·cm/cm(J/M)ft·lb/in bending strength ASTM D790/ISO 178 75 kg/cm²(MPa)[Lb/in²] elongation ASTM D638/ISO 527 2 % tensile strength ASTM D638/ISO 527 41屈服 32断裂 kg/cm²(MPa)[Lb/in²]
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Vicat softening temperature 1/8",50℃/hr,120℃/10hr ASTM D-1525 106 °C Vicat softening temperature ASTM D1525/ISO R306 92 ℃(℉)
Physical properties شرایط آزمون روش آزمون نتیجه آزمون melt mass-flow rate ASTM D1238/ISO 1133 3.9 g/10min
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.