Impact strength of simply supported beam without notch
23°C
ISO 179
NoBreak
flammability
شرایط آزمون
روش آزمون
نتیجه آزمون
UL flame retardant rating
2.5mm
UL 94
5VA
UL flame retardant rating
1.5mm
UL 94
5VB
UL flame retardant rating
1.2mm
UL 94
V-0
mechanical properties
شرایط آزمون
روش آزمون
نتیجه آزمون
bending strength
ASTM D790/ISO 178
820 kg/cm²(MPa)[Lb/in²]
Bending modulus
ASTM D790/ISO 178
25000 kg/cm²(MPa)[Lb/in²]
tensile strength
ASTM D638/ISO 527
560 kg/cm²(MPa)[Lb/in²]
Elongation at Break
ASTM D638/ISO 527
50 %
Impact strength of cantilever beam gap
ASTM D256/ISO 179
40 kg·cm/cm(J/M)ft·lb/in
bending strength
ISO 178
93.0 Mpa
Bending modulus
ISO 178
2600 Mpa
Tensile strain
Break
ISO 527-2/50
>20 %
tensile strength
Yield
ISO 527-2/50
62.0 Mpa
Tensile modulus
ISO 527-2/1
2500 Mpa
thermal performance
شرایط آزمون
روش آزمون
نتیجه آزمون
Combustibility (rate)
UL 94
V-0(1.5mm)
Vicat softening temperature
ISO 306/B50
99.0 °C
Hot deformation temperature
0.45MPa,Unannealed
ISO 75-2/B
91.0 °C
Physical properties
شرایط آزمون
روش آزمون
نتیجه آزمون
melt mass-flow rate
ASTM D1238/ISO 1133
20 g/10min
Shrinkage rate
ASTM D955
0.4-0.6 %
density
ASTM D792/ISO 1183
1.18
Shrinkage rate
MD
Internal Method
0.40-0.60 %
melt mass-flow rate
250°C/2.16kg
ISO 1133
20 g/10min