برگه داده فنی مقایسهimpact performance شرایط آزمون روش آزمون نتیجه آزمون Impact strength of cantilever beam gap Injection ASTM D256 75 J/m
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون bending strength Injection ASTM D790 25.0 Mpa Bending modulus Injection ASTM D790 1000 Mpa elongation Break,Injection ASTM D638 >800 % tensile strength Break,Injection ASTM D638 18.0 Mpa tensile strength Yield,Injection ASTM D638 26.0 Mpa Tensile modulus Injection,1%Secant ASTM D638 950 Mpa
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Vicat softening temperature ASTM D1525 125 °C Brittle temperature ASTM D746 <-75.0 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون density ASTM D1505 0.964 g/cm³ Environmental stress cracking resistance 100%Igepal,Compression Molded,F50 ASTM D1693B 3.00 hr Environmental stress cracking resistance 10%Igepal,Compression Molded,F50 ASTM D1693B 2.00 hr melt mass-flow rate 190°C/2.16kg ASTM D1238 8.0 g/10min
hardness شرایط آزمون روش آزمون نتیجه آزمون Shore hardness ShoreD,Injection ASTM D2240 62