برگه داده فنی مقایسهOther performance شرایط آزمون روش آزمون نتیجه آزمون Starting temperature of heat sealing Internal Method 92.8 ℃ Water vapor permeability 38℃,90% RH DIN 53122/2 g·mm/m
Basic Performance شرایط آزمون روش آزمون نتیجه آزمون Monomer content Internal Method %
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون tensile strength Yield,Compression Molded ASTM D-638 8.34 MPa tensile strength Yield,Compression Molded ISO 527-2 8.34 MPa tensile strength Compression Molded,Break ASTM D-638 17.4 MPa tensile strength Yield,Compression Molded ASTMD638 8.34 Mpa tensile strength Break,Compression Molded ASTMD638 17.4 Mpa elongation Break,Compression Molded ASTMD638 520 % tensile strength Compression Molded,Break ISO 527-2 17.4 MPa Elongation at Break Compression Molded ASTM D-638 520 % Elongation at Break Compression Molded ISO 527-2 520 %
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Vicat softening temperature ASTMD1525 85.0 °C Melting temperature Internal Method 100 °C Vicat softening temperature ASTM D-1525 85 ℃ Vicat softening temperature ISO 306 85 ℃
Physical properties شرایط آزمون روش آزمون نتیجه آزمون melt mass-flow rate 190°C/2.16kg ASTMD1238 5.8 g/10min Content of comonomer Internal Method 6.5 %
film شرایط آزمون روش آزمون نتیجه آزمون Initial sealing temperature Internal Method 92.8 °C Water vapor permeability 38°C,90%RH DIN 53122/2 0.40 g·mm/m²/atm/24hr