برگه داده فنی مقایسهelastomer شرایط آزمون روش آزمون نتیجه آزمون elongation Break,3.20mm ASTM D412 560 % tensile strength Break,3.20mm ASTM D412 32.0 Mpa tensile strength 300%Strain,3.20mm ASTM D412 12.1 Mpa tensile strength 100%Strain,3.20mm ASTM D412 6.90 Mpa tensile strength 50%Strain,3.20mm ASTM D412 5.50 Mpa Permanent compression deformation 70°C,22hr ASTM D395B 80 % Permanent compression deformation 25°C,22hr ASTM D395B 25 % tear strength 3.20mm ASTM D624 82.3 kN/m
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون Taber abraser 1000g,H-22Wheel ASTM D1044 5.00 mg
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Linear coefficient of thermal expansion MD ASTM D696 1.7E-04 cm/cm/°C Vicat softening temperature ASTM D15252 67.2 °C Glass transition temperature DSC -38.0 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون melt mass-flow rate 224°C/8.7kg ASTM D1238 24 g/10min Shrinkage rate MD ASTM D955 0.0-0.60 % Shrinkage rate TD ASTM D955 0.50-0.70 %
hardness شرایط آزمون روش آزمون نتیجه آزمون Shore hardness ShoreD ASTM D2240 48 Shore hardness ShoreA ASTM D2240 88
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.