Impact strength of simply supported beam without notch
23°C
ISO 179/1eU
NB kJ/m²
Impact strength of simply supported beam without notch
-30°C
ISO 179/1eU
150 kJ/m²
Elongation at Break
23°C
ISO 527-2
2.40 %
Tensile modulus
23°C
ISO 527-2
2200 Mpa
Charpy Notched Impact Strength
23°C
ISO 179/1eA
24 kJ/m²
Charpy Notched Impact Strength
-30°C
ISO 179/1eA
14 kJ/m²
thermal performance
شرایط آزمون
روش آزمون
نتیجه آزمون
Hot deformation temperature
0.45MPaUnannealed
ISO 75-2/Bf
96 °C
Hot deformation temperature
1.80MPaAnnealed
ISO 75-2/Af
94 °C
Vicat softening temperature
ISO 306/A50
95 °C
Linear coefficient of thermal expansion
MD
ISO 11359-2
0.00010 cm/cm/°C
Physical properties
شرایط آزمون
روش آزمون
نتیجه آزمون
melt mass-flow rate
220℃/10Kg
ISO 1133
25 cm3/10min
Electrical performance
شرایط آزمون
روش آزمون
نتیجه آزمون
Volume resistivity
IEC 60093
1E+13 Ω.cm
Dielectric strength
IEC 60243-1
18 KV/mm
Dielectric constant
IEC 60250
2.80 100HZ
Dissipation factor
IEC 60250
0.0050 100HZ
flame retardant performance
شرایط آزمون
روش آزمون
نتیجه آزمون
UL flame retardant rating
UL -94
HB 1.50mm
UL flame retardant rating
UL -94
HB 3.00mm