برگه داده فنی مقایسهmachinability شرایط آزمون روش آزمون نتیجه آزمون Screw speed 30-40 rpm Processing temperature 190-205 °C Processing temperature 185-195 °C Processing temperature 180-195 °C Processing temperature 160-175 °C Dry conditions 98℃ 2-3小时
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون Tensile modulus 100% ASTM D412/ISO 527 15 Mpa/Psi Tensile modulus 300% ASTM D412/ISO 527 27 Mpa/Psi tensile strength ASTM D412/ISO 527 47 Mpa/Psi tear strength ASTM D624/ISO 34 180 n/mm² Friction coefficient DIN 53516 60 mg Resilience ISO 4662 30 % tear strength ISP 34-1:2004(E) 180 kN/m elongation Break ISO 37 420 % tensile strength ISO 37 47 Mpa Tensile stress 300%伸长率 ISO 37 27 Mpa Tensile stress 100%伸长率 ISO 37:2005(E) 15 Mpa Resilience ASTM D2630/ISO 4662 30 % Shore hardness ASTM D2240/ISO 868 98 Shore A
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Glass transition temperature (Tg) ASTM D3417 -30 °C Vicat softening temperature ISO 306 125 °C Vicat softening temperature ASTM D1525/ISO R306 125 ℃(℉) Glass transition temperature ASTM D3418/ISO 815 -30 ℃(℉)
Physical properties شرایط آزمون روش آزمون نتیجه آزمون Shore hardness ISO 868:2006(E) 98±2/55 density ASTM D792/ISO 2781/JIS K7311 1.2
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.