برگه داده فنی مقایسهimpact performance شرایط آزمون روش آزمون نتیجه آزمون Impact strength of cantilever beam gap 23°C ISO 180/1A 9.0 kJ/m² Charpy Notched Impact Strength 23°C ISO 179/1eA 10 kJ/m²
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون Tensile modulus ASTM D638 2100 Mpa Tensile modulus ISO 527-2/50 2400 Mpa bending strength ISO 178 80.0 Mpa bending strength ASTM D790 70.0 Mpa Bending modulus ISO 178 2400 Mpa Bending modulus ASTM D790 2300 Mpa Tensile strain Break ISO 527-2/50 11 % elongation Break ASTM D638 17 % tensile strength Break ISO 527-2/50 40.0 Mpa tensile strength Break ASTM D638 36.0 Mpa tensile strength Yield ISO 527-2/50 52.0 Mpa tensile strength Yield ASTM D638 47.0 Mpa
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Vicat softening temperature ISO 306/B50 104 °C Hot deformation temperature 1.8MPa,Annealed,4.00mm ISO 75-2/A 103 °C Hot deformation temperature 1.8MPa,Unannealed,4.00mm ISO 75-2/A 82.0 °C Hot deformation temperature 1.8MPa,Unannealed,6.40mm ASTM D648 93.0 °C Hot deformation temperature 0.45MPa,Annealed,4.00mm ISO 75-2/B 107 °C Hot deformation temperature 0.45MPa,Unannealed,4.00mm ISO 75-2/B 97.0 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون Shrinkage rate TD:3.20mm ISO 2577 0.40-0.70 % Shrinkage rate MD:3.20mm ISO 2577 0.40-0.70 % Shrinkage rate TD:3.20mm ASTM D955 0.40-0.70 % Shrinkage rate MD:3.20mm ASTM D955 0.40-0.70 % melt mass-flow rate 220°C/10.0kg ISO 1133 5.0 g/10min melt mass-flow rate 220°C/10.0kg ASTM D1238 5.0 g/10min
hardness شرایط آزمون روش آزمون نتیجه آزمون Rockwell hardness R-Scale ISO 2039-2 108 Rockwell hardness R-Scale ASTM D785 107