برگه داده فنی مقایسهCONDITION شرایط آزمون روش آزمون نتیجه آزمون Pre drying temperature - 70~80 ℃ Pre drying time - 3~4 hrs Temperature - 200~250 ℃ Mold temperature - 40~80 ℃ Screw speed - 30~60 rpm
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون tensile strength Yield,23℃, 50mm/min, 3.2mm ASTM D638 42 Mpa Elongation at Break 23℃, 50mm/min, 3.2mm ASTM D638 ≥10 % bending strength 23℃, 10mm/min, 6.4mm ASTM D790 70 Mpa Bending modulus 23℃, 10mm/min, 6.4mm ASTM D790 2350 Mpa Izod Notched Impact Strength Notched, 3.2mm, 23℃ ASTM D256 270 J/m Izod Notched Impact Strength Notched, 6.4mm, 23℃ ASTM D256 250 J/m
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Hot deformation temperature Edgewise,1.82MPa,6.4mm,Unannealed ASTM D648 85 ℃ Vicat softening temperature 50N, 50℃/h ASTM D1525 93 ℃
Physical properties شرایط آزمون روش آزمون نتیجه آزمون density 23℃ ASTM D792 1.04 g/cm³ Shrinkage rate 23℃, 3.2mm ASTM D955 0.4~0.7 % melt mass-flow rate 220℃, 10kg ASTM D1238 40 g/10min
hardness شرایط آزمون روش آزمون نتیجه آزمون Rockwell hardness ASTM D785 106 R
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.