برگه داده فنی مقایسهmachinability شرایط آزمون روش آزمون نتیجه آزمون Mold temperature 20-30 °C Processing temperature 180-190 °C Processing temperature 170-180 °C Processing temperature 175-185 °C Processing temperature 140-160 °C Dry conditions 85℃ 3小时
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون Friction coefficient DIN 53516 27 mg Resilience ISO 4662 45 % tear strength ISP 34-1:2004(E) 110 kN/m elongation Break ISO 37 520 % tensile strength ISO 37 40 Mpa Tensile stress 300%伸长率 ISO 37 11 Mpa Tensile stress 100%伸长率 ISO 37:2005(E) 6.0 Mpa Resilience ASTM D2630/ISO 4662 45 % Shore hardness ASTM D2240/ISO 868 85+_2 Shore A tear strength ASTM D624/ISO 34 110 n/mm² tensile strength ASTM D412/ISO 527 40 Mpa/Psi Tensile modulus 300% ASTM D412/ISO 527 11 Mpa/Psi Tensile modulus 100% ASTM D412/ISO 527 6.0 Mpa/Psi
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Glass transition temperature (Tg) ASTM D3417 -40 °C Vicat softening temperature ISO 306 100 °C Vicat softening temperature ASTM D1525/ISO R306 100 ℃(℉) Glass transition temperature ASTM D3418/ISO 815 -40 ℃(℉)
Physical properties شرایط آزمون روش آزمون نتیجه آزمون Shore hardness ISO 868:2006(E) 85±2/- density ASTM D792/ISO 2781/JIS K7311 1.19
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.