Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 J-1/30/TF/15 DSM HOLAND
--
Cam,Pulley,bearing,Engine parts
Filler: Glass fiber reinf,30% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | DSM HOLAND/J-1/30/TF/15 |
|---|---|---|---|
| Rockwell hardness | R-Scale | ASTM D785 | 119 |
| thermal performance | Test Condition | Test Method | DSM HOLAND/J-1/30/TF/15 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 254 °C |
| 0.45MPa,Unannealed | ASTM D648 | 260 °C | |
| 0.45MPa | ISO 75-22 | 260 °C | |
| 1.8MPa | ISO 75-22 | 250 °C | |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 4.3E-05 cm/cm/°C |
| Melting temperature | ISO 11357-32 | 260 °C | |
| RTI Elec | 1.5mm | UL 746 | 65.0 °C |
| RTI Imp | 1.5mm | UL 746 | 65.0 °C |
| RTI Str | 1.5mm | UL 746 | 65.0 °C |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/J-1/30/TF/15 |
|---|---|---|---|
| Bending modulus | 23°C | ASTM D790 | 9310 Mpa |
| bending strength | Break,23°C | ASTM D790 | 238 Mpa |
| ASTM D790 | 238 Mpa | ||
| compressive strength | ASTM D695 | 193 Mpa | |
| elongation | Break | ASTM D638 | 2.5 % |
| Friction coefficient | Steel - Dynamic | ASTM D1894 | 0.25 |
| Steel - Static6 | ASTM D1894 | 0.20 | |
| shear strength | ASTM D732 | 68.9 Mpa | |
| Tensile modulus | ISO 527-22 | 9000 Mpa | |
| Tensile strain | Break | ISO 527-22 | 2.5 % |
| tensile strength | Break | ISO 527-22 | 160 Mpa |
| ASTM D638 | 159 Mpa |
| Physical properties | Test Condition | Test Method | DSM HOLAND/J-1/30/TF/15 |
|---|---|---|---|
| Shrinkage rate | MD:3.18mm | ASTM D955 | 0.20 % |
| Water absorption rate | Saturation | ISO 622 | 5.3 % |
| Equilibrium | ISO 622 | 1.4 % | |
| 24hr | ASTM D570 | 0.60 % |
| impact performance | Test Condition | Test Method | DSM HOLAND/J-1/30/TF/15 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA2 | 10.0 kJ/m² |
| flammability | Test Condition | Test Method | DSM HOLAND/J-1/30/TF/15 |
|---|---|---|---|
| Burning Behav.atthicknessh | 1.50mm,UL | HB 4.21 | |
| Normal combustion performance with a thickness of 1.6mm | 1.50mm,UL | HB 4.21 | |
| UL flame retardant rating | 1.6mm | UL 94 | HB |