ABS 730GS DOW JAPAN
CELEX™
--
Filler: Glass fiber reinf,30%,Filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | DOW JAPAN/730GS |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTM D648 | 100 °C |
| mechanical properties | Test Condition | Test Method | DOW JAPAN/730GS |
|---|---|---|---|
| Bending modulus | 3.20mm | ASTM D790 | 6100 Mpa |
| bending strength | 3.20mm | ASTM D790 | 108 Mpa |
| Tensile modulus | 3.20mm | ASTM D638 | 5350 Mpa |
| tensile strength | Yield,3.20mm | ASTM D638 | 86.0 Mpa |
| Physical properties | Test Condition | Test Method | DOW JAPAN/730GS |
|---|---|---|---|
| melt mass-flow rate | 230°C/3.8kg | ASTM D1238 | 3.0 g/10min |
| Shrinkage rate | MD:3.20mm | ASTM D955 | 0.20-0.40 % |