POM GH-25D CD3501 JAPAN POLYPLASTIC
DURACON®
Automotive Applications,Fitness equipment
High impact resistance,High mobility,Filler: Glass fiber reinf,25% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | JAPAN POLYPLASTIC/GH-25D CD3501 |
|---|---|---|---|
| Rockwell hardness | M-Scale | ISO 2039-2 | 95 |
| Supplementary Information | Test Condition | Test Method | JAPAN POLYPLASTIC/GH-25D CD3501 |
|---|---|---|---|
| ColourNumber | CF3500/CD3501 |
| thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/GH-25D CD3501 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 162 °C |
| Linear coefficient of thermal expansion | MD:23to55°C | Internal Method | 3E-05 cm/cm/°C |
| TD:23to55°C | Internal Method | 9E-05 cm/cm/°C |
| mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/GH-25D CD3501 |
|---|---|---|---|
| Bending modulus | ISO 178 | 7900 Mpa | |
| bending strength | ISO 178 | 196 Mpa | |
| Friction coefficient | Dynamic2 | JISK7218 | 0.37 |
| Steel - Dynamic3 | JISK7218 | 0.60 | |
| Tensile modulus | ISO 527-2 | 8500 Mpa | |
| Tensile strain | Break | ISO 527-2 | 2.4 % |
| tensile strength | ISO 527-2 | 136 Mpa | |
| Wear factor | 0.060MPa,0.15m/sec4 | JISK7218 | 300 10^-8mm³/N·m |
| 0.49MPa,0.30m/sec5 | JISK7218 | 400 10^-8mm³/N·m | |
| 0.060MPa,0.15m/sec7 | JISK7218 | 10000 10^-8mm³/N·m | |
| 0.49MPa,0.30m/sec6 | JISK7218 | 7000 10^-8mm³/N·m |
| Electrical performance | Test Condition | Test Method | JAPAN POLYPLASTIC/GH-25D CD3501 |
|---|---|---|---|
| Dielectric strength | 3.00mm | IEC 60243-1 | 24 KV/mm |
| Surface resistivity | IEC 60093 | 4E+16 ohms | |
| Volume resistivity | IEC 60093 | 5E+13 ohms·cm |
| Physical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/GH-25D CD3501 |
|---|---|---|---|
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 12 g/10min |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 9.00 cm3/10min |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.60 % |
| flammability | Test Condition | Test Method | JAPAN POLYPLASTIC/GH-25D CD3501 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |