Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 408L DUPONT JAPAN
Zytel®
Non specific food applications
--
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | DUPONT JAPAN/408L |
|---|---|---|---|
| EmissionofOrganicCompounds | VDA277 | 35.0 µgC/g | |
| Odor | VDA270 | 4.00 |
| thermal performance | Test Condition | Test Method | DUPONT JAPAN/408L |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 155 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 66.0 °C | |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1.3E-04 cm/cm/°C |
| MD | ISO 11359-2 | 1.3E-04 cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 263 °C | |
| Vicat softening temperature | ISO 306/B50 | 210 °C |
| film | Test Condition | Test Method | DUPONT JAPAN/408L |
|---|---|---|---|
| Tensile strain | Yield,MD | ISO 527-3 | 6.0 % |
| mechanical properties | Test Condition | Test Method | DUPONT JAPAN/408L |
|---|---|---|---|
| Nominal tensile fracture strain | ISO 527-2 | 35 % | |
| Tensile creep modulus | 1hr | ISO 899-1 | -- Mpa |
| 1000hr | ISO 899-1 | -- Mpa | |
| Tensile modulus | ISO 527-2 | 2200 Mpa | |
| Tensile strain | Yield | ISO 527-2 | 6.0 % |
| tensile strength | Yield | ISO 527-2 | 61.0 Mpa |
| Electrical performance | Test Condition | Test Method | DUPONT JAPAN/408L |
|---|---|---|---|
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 | |
| Dielectric strength | IEC 60243-1 | 34 KV/mm | |
| Dissipation factor | 1MHz | IEC 60250 | 0.020 |
| 100Hz | IEC 60250 | 0.020 | |
| Relative permittivity | 100Hz | IEC 60250 | 3.20 |
| 1MHz | IEC 60250 | 2.90 | |
| Surface resistivity | IEC 60093 | -- ohms | |
| Volume resistivity | IEC 60093 | >1.0E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | DUPONT JAPAN/408L |
|---|---|---|---|
| density | ISO 1183 | 1.09 g/cm³ | |
| MediumDensity | 0.950 g/cm³ | ||
| Shrinkage rate | MD | ISO 294-4 | 1.5 % |
| TD | ISO 294-4 | 1.5 % | |
| SpecificHeatCapacity of Melt | 2600 J/kg/°C | ||
| ThermalConductivityofMelt | 0.16 W/m/K | ||
| Top out temperature | 190 °C | ||
| Water absorption rate | Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 2.2 % |
| Saturation,23°C,2.00mm | ISO 62 | 7.0 % |
| impact performance | Test Condition | Test Method | DUPONT JAPAN/408L |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 15 kJ/m² |
| -30°C | ISO 179/1eA | 15 kJ/m² | |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | NoBreak |
| 23°C | ISO 179/1eU | NoBreak |
| flammability | Test Condition | Test Method | DUPONT JAPAN/408L |
|---|---|---|---|
| Burning rate | 1.00mm | ISO 3795 | <100 mm/min |
| Extreme Oxygen Index | ISO 4589-2 | 19 % | |
| FMVSS flammability | FMVSS302 | B | |
| UL flame retardant rating | 0.75mm | UL 94 | HB |
| 0.75mm | IEC 60695-11-10,-20 | HB | |
| 1.5mm | IEC 60695-11-10,-20 | HB | |
| 1.5mm | UL 94 | HB |