PA66 A3K Q722 BASF GERMANY
Ultramid®
Electrical field,Electronic field,Industrial machinery,Industrial applications,Electronic insulation
High mobility,Oil resistant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Basic Performance | Test Condition | Test Method | BASF GERMANY/A3K Q722 |
|---|---|---|---|
| density | ISO 1183 | 1130 Kg/m | |
| Water absorption rate | Equilibrium | ISO 62 | 2.8 % |
| Saturation | ISO 62 | 8.5 % |
| thermal performance | Test Condition | Test Method | BASF GERMANY/A3K Q722 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa | ISO 75-2 | 75 ℃ |
| 0.45MPa,Unannealed | ISO 75-2/B | 200 °C | |
| 1.8MPa,Unannealed | ISO 75-2/A | 75.0 °C | |
| Melting temperature | ISO 3146 | 260 °C | |
| DSC | ISO 3146 | 260 ℃ |
| mechanical properties | Test Condition | Test Method | BASF GERMANY/A3K Q722 |
|---|---|---|---|
| Impact strength of simply supported beam without notch | 23℃ | ISO 179/1eA | 5 KJ/m |
| Tensile modulus | 23°C | ISO 527-2 | 3600 Mpa |
| ISO 527-2 | 3600 MPa | ||
| Tensile strain | Yield | ISO 527-2 | 4.2 % |
| Yield,23°C | ISO 527-2 | 4.2 % | |
| tensile strength | Yield | ISO 527-2 | 87 MPa |
| Yield,23°C | ISO 527-2 | 87.0 Mpa |
| Physical properties | Test Condition | Test Method | BASF GERMANY/A3K Q722 |
|---|---|---|---|
| density | ISO 1183 | 1.13 g/cm³ | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 2.8 % |
| Saturation,23°C | ISO 62 | 8.5 % |
| impact performance | Test Condition | Test Method | BASF GERMANY/A3K Q722 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179 | 5.0 kJ/m² |