PPO GFN2V-960 SABIC INNOVATIVE US
NORYL™
Household appliances,Household appliances,Fitness equipment,Automotive interior parts
enhance,Glass fiber reinforced, Glass fiber reinforced
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Basic Performance | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2V-960 |
|---|---|---|---|
| Water absorption rate | 24hrs | ASTM D-570 | 0.06 % |
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2V-960 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa | ASTM D-648 | 132 °C |
| 0.45MPa | ASTM D-648 | 137 °C | |
| Linear coefficient of thermal expansion | ASTM E-831 | 3.6×10 1/°C | |
| Long term use temperature | 电气 | UL 746B | 110 °C |
| 含冲击 | UL 746B | 105 °C | |
| 无冲击 | UL 746B | 110 °C |
| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2V-960 |
|---|---|---|---|
| Bending modulus | 6.4mm | ASTM D-790 | 5719 Mpa |
| bending strength | 6.4mm | ASTM D-790 | 152 Mpa |
| Impact strength of cantilever beam gap | 23°C | ASTM D-256 | 107 J/m |
| -40°C | ASTM D-256 | 96 J/m | |
| Rockwell hardness | ASTM D-785 | 106 | |
| tensile strength | Yield点,3.2mm | ASTM D-638 | 107 Mpa |
| Break点,3.2mm | ASTM D-638 | 5 Mpa |
| Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2V-960 |
|---|---|---|---|
| Dielectric constant | 60Hz | ASTM D-150 | 2.98 |
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2V-960 |
|---|---|---|---|
| density | ASTM D-792 | 1.23 | |
| Dissipation factor | 60Hz | ASTM D-150 | 0.0016 |
| enhance | 20 % | ||
| Shrinkage rate | 3.2mm | ASTM D-955 | 2-5 10 |
| UL flame retardant rating | UL 94 | V-1 | |
| UL 94 | 1.5 mm |