PBT 361SA ED3002 JAPAN POLYPLASTIC
DURANEX®
Automotive Applications
Glass fiber reinforced,Filler: Glass fiber reinf,15% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | JAPAN POLYPLASTIC/361SA ED3002 |
|---|---|---|---|
| ColourNumber | ED3002 |
| hardness | Test Condition | Test Method | JAPAN POLYPLASTIC/361SA ED3002 |
|---|---|---|---|
| Rockwell hardness | M-Scale | ISO 2039-2 | 75 |
| thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/361SA ED3002 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 125 °C |
| Linear coefficient of thermal expansion | MD:23to55°C | Internal Method | 4E-05 cm/cm/°C |
| TD:23to55°C | Internal Method | 8E-05 cm/cm/°C |
| mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/361SA ED3002 |
|---|---|---|---|
| Bending modulus | ISO 178 | 5700 Mpa | |
| bending strength | ISO 178 | 129 Mpa | |
| Tensile strain | Break | ISO 527-2 | 2.1 % |
| tensile strength | ISO 527-2 | 90.0 Mpa |
| Electrical performance | Test Condition | Test Method | JAPAN POLYPLASTIC/361SA ED3002 |
|---|---|---|---|
| Dielectric strength | 3.00mm | IEC 60243-1 | 20 KV/mm |
| Volume resistivity | IEC 60093 | 2E+16 ohms·cm |
| Physical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/361SA ED3002 |
|---|---|---|---|
| Water absorption rate | 23°C,24hr | ISO 62 | 0.20 % |
| flammability | Test Condition | Test Method | JAPAN POLYPLASTIC/361SA ED3002 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | V-0 |