Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM WR-01 JAPAN POLYPLASTIC
DURACON®
Electronic and electrical components
Low moisture absorption
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | JAPAN POLYPLASTIC/WR-01 |
|---|---|---|---|
| Rockwell hardness | M-Scale | ISO 2039-2 | 80 |
| Supplementary Information | Test Condition | Test Method | JAPAN POLYPLASTIC/WR-01 |
|---|---|---|---|
| ColourNumber | CF2001 |
| thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/WR-01 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 78.0 °C |
| Linear coefficient of thermal expansion | MD:23to55°C | Internal Method | 1.2E-04 cm/cm/°C |
| TD:23to55°C | Internal Method | 1.2E-04 cm/cm/°C |
| mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/WR-01 |
|---|---|---|---|
| Bending modulus | ISO 178 | 2200 Mpa | |
| bending strength | ISO 178 | 76.0 Mpa | |
| Friction coefficient | Dynamic2 | JISK7218 | 0.25 |
| Steel - Dynamic3 | JISK7218 | 0.19 | |
| Nominal tensile fracture strain | ISO 527-2 | 38 % | |
| Tensile modulus | ISO 527-2 | 2400 Mpa | |
| tensile strength | ISO 527-2 | 58.0 Mpa | |
| Wear factor | 0.98MPa,0.30m/sec4 | JISK7218 | <1.0 10^-8mm³/N·m |
| 0.98MPa,0.30m/sec5 | JISK7218 | 20 10^-8mm³/N·m | |
| 0.060MPa,0.15m/sec6 | JISK7218 | 3500 10^-8mm³/N·m | |
| 0.060MPa,0.15m/sec7 | JISK7218 | 10000 10^-8mm³/N·m |
| Electrical performance | Test Condition | Test Method | JAPAN POLYPLASTIC/WR-01 |
|---|---|---|---|
| Dielectric strength | 3.00mm | IEC 60243-1 | 19 KV/mm |
| Surface resistivity | IEC 60093 | 5E+13 ohms | |
| Volume resistivity | IEC 60093 | 1E+13 ohms·cm |
| Physical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/WR-01 |
|---|---|---|---|
| density | ISO 1183 | 1.41 g/cm³ | |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 10 g/10min |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 8.00 cm3/10min |
| Shrinkage rate | TD:2.00mm | ISO 294-4 | 1.8 % |
| MD:2.00mm | ISO 294-4 | 2.1 % | |
| Water absorption rate | 23°C,24hr | ISO 62 | 1.2 % |
| impact performance | Test Condition | Test Method | JAPAN POLYPLASTIC/WR-01 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 5.6 kJ/m² |