Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD | ASTMD995 | 0.20 | % |
Modeling Shrinkage | TD | ASTMD995 | 0.80 | % |
Moisture Absorption | | ASTMD570 | 0.050 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | 23°C | ASTMD638 | 110 | Mpa |
Tensile Elongation (Break) | 23°C | ASTMD638 | 1.5 | % |
Flexural Strength | 23°C | ASTMD790 | 150 | Mpa |
Flexural Modulus | 23°C | ASTMD790 | 13000 | Mpa |
Notched Izod Impact Strength | 23°C | ASTMD256 | 63.0 | J/m |
Notched Izod Impact Strength | 泰伯磨耗试验 | ASTMD1044 | 38 | mg/1000cycles |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Heat Deflection Temperature | 0.45MPaUnannealed | ASTMD648 | 240 | °C |
Heat Deflection Temperature | 1.80MPaUnannealed | ASTMD648 | 225 | °C |
Coefficient of Linear Thermal Expansion | MD | ASTMD696 | 2.5E-05 | cm/cm/°C |
Coefficient of Linear Thermal Expansion | 熔点 | | 255 | °C |
Coefficient of Linear Thermal Expansion | 最大使用温度 | ASTMUL746B | 130 | °C |
Electrical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Volume Resistivity | | ASTMD257 | 1E+14 | Ω.cm |
Insulation Resistance | 2.00mm | ASTMD149 | 36 | KV/mm |
Dissipation Factor | 耐电弧性 | ASTMD495 | 181 | S |
Hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | | ASTMD785 | 90 | M(Scale) |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.