POM/PTFE LNP™ LUBRICOMP™ KL-4040-NAT SABIC INNOVATIVE US
33
- Unit Price:
- $4973 USD/MT
- Packaging Specification:
- 25KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:24hr | ASTMD955 | 2.0to2.5 | % |
TD:24hr | ASTMD955 | 2.0to2.5 | % | |
TD:24hr | ISO294-4 | 2.0to2.5 | % | |
MD:24hr | ISO294-4 | 2.0to2.5 | % | |
Moisture Absorption | 24hr,50%RH | ASTMD570 | 0.15 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.26 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Modulus | ASTMD638 | 2140 | Mpa | |
Tensile Modulus | ISO527-2/1 | 2400 | Mpa | |
Tensile Strength | Yield | ASTMD638 | 51.1 | Mpa |
Tensile Stress | Yield | ISO527-2 | 47.3 | Mpa |
Tensile Strength | Break | ASTMD638 | 50.9 | Mpa |
Tensile Stress | Break | ISO527-2 | 46.5 | Mpa |
Tensile Elongation | Yield | ASTMD638 | 11 | % |
Tensile Strain | Yield | ISO527-2 | 10 | % |
Tensile Elongation | Break | ASTMD638 | 18 | % |
Tensile Strain | Break | ISO527-2 | 23 | % |
Flexural Modulus | ASTMD790 | 2070 | Mpa | |
ISO178 | 2600 | Mpa | ||
Flexural Strength | ASTMD790 | 75.8 | Mpa | |
Flexural Stress | ISO178 | 79.3 | Mpa | |
Coefficient of Friction | Dynamic | ASTMD3702Modified | 0.29 | |
Static | ASTMD3702Modified | 0.15 | ||
Specific Wear Rate | ASTMD3702Modified | 15.0 | 10^-10in^5-min/ft-lb-hr |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Coefficient of Linear Thermal Expansion | TD:-40to40°C | ASTME831 | 1.1E-04 | cm/cm/°C |
TD:-40to40°C | ISO11359-2 | 1.1E-04 | cm/cm/°C | |
Heat Deflection Temperature | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 157 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 99.4 | °C | |
Heat Deflection Temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 98.0 | °C |
Coefficient of Linear Thermal Expansion | MD:-40to40°C | ASTME831 | 1.1E-04 | cm/cm/°C |
MD:-40to40°C | ISO11359-2 | 1.1E-04 | cm/cm/°C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod Impact Strength | 23°C | ISO180/1A | 4.0 | kJ/m² |
UnnotchedIzodImpactStrength3 | 23°C | ISO180/1U | 45 | kJ/m² |
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 6.40 | J |
Multi-Axial Instrumented Impact Energy | ISO6603-2 | 0.770 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.