Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD | ASTMD955 | 0.50to0.70 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Modulus | 23°C | ASTMD638 | 1580 | Mpa |
Tensile Modulus | 23°C | ISO527-2 | 1600 | Mpa |
Tensile Strength | Yield,23°C | ASTMD638 | 43.0 | Mpa |
Tensile Stress | Yield,23°C | ISO527-2 | 44.0 | Mpa |
Tensile Strength | Break,23°C | ASTMD638 | 52.0 | Mpa |
Tensile Stress | Break,23°C | ISO527-2 | 49.0 | Mpa |
Tensile Elongation | Yield,23°C | ASTMD638 | 7.0 | % |
Tensile Strain | Yield,23°C | ISO527-2 | 7.0 | % |
Tensile Strain | Break,23°C | ISO527-2 | 150 | % |
Flexural Modulus | 23°C | ASTMD790 | 1580 | Mpa |
Flexural Modulus | 23°C | ISO178 | 1500 | Mpa |
Flexural Stress | 23°C | ISO178 | 60.0 | Mpa |
Flexural Strength | Yield,23°C | ASTMD790 | 64.0 | Mpa |
Tensile Elongation | Break,23°C | ASTMD638 | 210 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Heat Deflection Temperature | 0.45MPa,Unannealed | ASTMD648 | 94.0 | °C |
Heat Deflection Temperature | 1.8MPa,Unannealed | ASTMD648 | 81.0 | °C |
Hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | R-Sale,23°C | ASTMD785 | 111 | |
Optical | Test Condition | Test Method | Test Result | Unit |
---|
Light Transmittance | Total | ASTMD1003 | 91.0 | % |
Haze | | ASTMD1003 | <1.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.